ALLOY / UGIREX C

ALLOY / UGIREX C

Alloys Co-Cr for ceramic

Composition %:

Co: 62,0    Cr: 31,0    Mo: 4,0    Si: 2,2

 

  • Density: 8,6 g/cm³
  • Melting range: 1210 - 1370 °C
  • C.E.T (25-500/25/600°C): 14,4 - 14,9 x 10-6 K-1
  • Casting temperature: 1470°C
  • Modulus of elasticity: 220 Gpa
  • Yiel strenght: 510 - 540 Mpa
  • Elongation: 12 - 7 %
  • Tensile strenght: 590 - 600 Mpa
  • Vickers hardness: 290 - 300 HV10