ALLOY / UGIREX C2

ALLOY / UGIREX C2

Alloys Co-Cr for ceramic

Composition %:

Co: 59,5    Cr: 31,5    Mo: 5,0    Si: 2,0

 

  • Density: 8,8 g/cm³
  • Melting range: 1240 - 1350 °C
  • C.E.T (25-500/25/600°C): 14,3 - 14,8 x 10-6 K-1
  • Casting temperature: 1480°C
  • Modulus of elasticity: -
  • Yiel strenght: 450 Mpa
  • Elongation: 9 %
  • Tensile strenght: 765 Mpa
  • Vickers hardness: 280 HV10